note: A: is printing material : B: pvc core
Producing procedure
1. Mirror-print the image on the printing material, dry the ink completely (normally around 5-10 minutes)
2. Remove the protection film on the middle material, put the printed material right on both side of the middle material, then, go through the laminator (set temperature around
3. Cut the laminated sheet into standard card, remove the protection film from the surface of the card.